Hlavní stránka>15/30322265 DC BS EN 3475-414. Aerospace series. Cables, electrical, aircraft use. Test methods. Part 414. Differential scanning calorimeter (DSC test)
Sponsored link
sklademVydáno: 2015-03-13
15/30322265 DC BS EN 3475-414. Aerospace series. Cables, electrical, aircraft use. Test methods. Part 414. Differential scanning calorimeter (DSC test)

15/30322265 DC

BS EN 3475-414. Aerospace series. Cables, electrical, aircraft use. Test methods. Part 414. Differential scanning calorimeter (DSC test)

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
600 Kč
Anglicky Tisk
Skladem
600 Kč
Označení normy:15/30322265 DC
Počet stran:6
Vydáno:2015-03-13
Status:Draft for Comment
Alternativní označení:BS EN 3475-414
Popis

15/30322265 DC


This standard 15/30322265 DC BS EN 3475-414. Aerospace series. Cables, electrical, aircraft use. Test methods. Part 414. Differential scanning calorimeter (DSC test) is classified in these ICS categories:
  • 49.025.40 Rubber and plastics
  • 49.060 Aerospace electric equipment and systems
  • 49.025.01 Materials for aerospace construction in general
  • 49.025.10 Steels
  • 49.025.99 Other materials
  • 19.040 Environmental testing
  • 25.220.20 Surface treatment