Vážení zákazníci, v letošním roce budeme expedovat poslední objednávky ve středu 18. 12. 2024.

Těšíme se s vámi na shledanou od pondělí 06. 01. 2025.

 

Cena s DPH / bez DPH
Hlavní stránka>BS 2782-10:Method 1003:1977 Methods of testing plastics. Glass reinforced plastics Determination of tensile properties
Sponsored link
sklademVydáno: 1977-08-31
BS 2782-10:Method 1003:1977 Methods of testing plastics. Glass reinforced plastics Determination of tensile properties

BS 2782-10:Method 1003:1977

Methods of testing plastics. Glass reinforced plastics Determination of tensile properties

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
4898 Kč
Čtěte normu po dobu 1 hodiny. Více informací v kategorii E-READING
Čtení normy
na 1 hodinu
489.80 Kč
Čtěte normu po dobu 24 hodin. Více informací v kategorii E-READING
Čtení normy
na 24 hodin
1469.40 Kč
Anglicky Tisk
Skladem
4898 Kč
Označení normy:BS 2782-10:Method 1003:1977
Počet stran:16
Vydáno:1977-08-31
ISBN:0 580 09735 8
Status:Standard
Popis

BS 2782-10:Method 1003:1977


This standard BS 2782-10:Method 1003:1977 Methods of testing plastics. Glass reinforced plastics is classified in these ICS categories:
  • 83.120 Reinforced plastics

1.1 This European Standard specifies a method of determining certain tensile properties of textile glass reinforced plastics. The method specified is not necessarily applicable to materials of very high tensile strength, for example unidirectional reinforced materials1). The method is applicable to reinforced thermosetting resins and also to reinforced thermoplastics.

Injection-moulded test specimens made from reinforced thermoplastics are subject to fibre orientation, and may give values that are untypically high; however, they may be used if other methods of specimen preparation are impracticable.

1.2 The method describes the determination of the following tensile properties:

  • the initial tangent modulus of elasticity and the tensile secant modulus of elasticity (when it is not possible to determine the initial tangent modulus of elasticity, the tensile secant modulus of elasticity at 0.1 % strain is determined);

  • maximum tensile stress;

NOTE If there is a clean break the maximum tensile stress is the stress at break; in other cases it is the stress corresponding to the maximum force.

  • the elongation at maximum force and, possibly, the elongation at break.

The force-elongation curves at different temperatures, degrees of humidity and rates of strain yield interesting information concerning the behaviour of the materials.

1.3 It is only possible to obtain comparable values between different materials if identical test specimens are used. These should also be tested under well defined conditions of pretreatment, temperature, humidity and rate of strain.

Finally, it is the aim of this method to obtain tensile results that can be used either for

  • quality control, or

  • the preparation of specifications for materials.