sklademVydáno: 1986-12-31
BS 6783-1:1986 Sampling and analysis of nickel, ferronickel and nickel alloys Method for determination of silver, bismuth, cadmium, cobalt, copper, iron, manganese, lead and zinc in nickel by flame atomic absorption spectrometry

BS 6783-1:1986

Sampling and analysis of nickel, ferronickel and nickel alloys Method for determination of silver, bismuth, cadmium, cobalt, copper, iron, manganese, lead and zinc in nickel by flame atomic absorption spectrometry

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
4898 Kč
Čtěte normu po dobu 1 hodiny. Více informací v kategorii E-READING
Čtení normy
na 1 hodinu
489.80 Kč
Čtěte normu po dobu 24 hodin. Více informací v kategorii E-READING
Čtení normy
na 24 hodin
1469.40 Kč
Anglicky Tisk
Skladem
4898 Kč
Označení normy:BS 6783-1:1986
Počet stran:16
Vydáno:1986-12-31
ISBN:0 580 15520 X
Status:Standard
Popis

BS 6783-1:1986


This standard BS 6783-1:1986 Sampling and analysis of nickel, ferronickel and nickel alloys is classified in these ICS categories:
  • 77.120.40 Nickel, chromium and their alloys

This International Standard specifies a flame atomic absorption spectrometric method for the determination of the silver, bismuth, cadmium, cobalt, copper, iron, manganese, lead and zinc contents of refined, wrought and cast nickel within the ranges specified in Table 1. This method is applicable to the independent determination of any one or more of the elements listed without including all the elements specified in the standard solutions.

Table 1 – Concentration ranges of elements to be determined

Element Concentration range, [% (m/m)]a
Procedure A Procedure B
Ag 0,000 2 to 0,01
Bi 0,000 1 to 0,01
Cd 0,000 2 to 0,002 5
Co 0,001 0 to 0,01 to 1,00
Cu 0,000 2 to 0,01 0,01 to 1,00
Fe 0,002 5 to 0,01 0,01 to 0,15
Mn 0,000 5 to 0,01 0,01 to 0,20
Pb 0,000 5 to 0,01
Zn 0,000 2 to 0,002 5 0,00 1 to 0,01 5
a For specific compositions, see ISO 6283.

The lower level for iron can be extended to less than 0,002 5 % (m/m) provided nickel containing less than 0,000 1 % (m/m) iron is used for preparation of standard solutions; see 4.1.

The upper limit for the determination of cobalt and copper can be raised to 2 % (m/m) by a minor modification to the method; see 11.1.

For potential interferences, see clause 10.