Cena s DPH / bez DPH
Hlavní stránka>BS EN 1011-8:2018 Welding. Recommendations for welding of metallic materials Welding of cast irons
Sponsored link
sklademVydáno: 2018-05-15
BS EN 1011-8:2018 Welding. Recommendations for welding of metallic materials Welding of cast irons

BS EN 1011-8:2018

Welding. Recommendations for welding of metallic materials Welding of cast irons

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
6600 Kč
Anglicky Tisk
Skladem
6600 Kč
Označení normy:BS EN 1011-8:2018
Počet stran:28
Vydáno:2018-05-15
ISBN:978 0 580 93116 1
Status:Standard
Popis

BS EN 1011-8:2018


This standard BS EN 1011-8:2018 Welding. Recommendations for welding of metallic materials is classified in these ICS categories:
  • 25.160.10 Welding processes
This document specifies the requirements for fusion welding of unalloyed and low-alloy cast iron castings produced in accordance with: - EN 1561, Founding - Grey cast irons; - EN 1562, Founding - Malleable cast irons; - EN 1563, Founding - Spheroidal graphite cast irons. This document does not apply to the joint welding of cast iron castings to other materials.