BS EN ISO 11463:2020 Corrosion of metals and alloys. Guidelines for the evaluation of pitting corrosion

BS EN ISO 11463:2020

Corrosion of metals and alloys. Guidelines for the evaluation of pitting corrosion

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
4740 Kč
Anglicky Tisk
Skladem
4740 Kč
Označení normy:BS EN ISO 11463:2020
Počet stran:22
Vydáno:2020-09-14
ISBN:978 0 580 97898 2
Status:Standard
Popis

BS EN ISO 11463:2020


This standard BS EN ISO 11463:2020 Corrosion of metals and alloys. Guidelines for the evaluation of pitting corrosion is classified in these ICS categories:
  • 77.060 Corrosion of metals

This document gives guidelines for the selection of procedures that can be used in the identification and examination of corrosion pits and in the evaluation of pitting corrosion and pit growth rate.