Cena s DPH / bez DPH
Hlavní stránka>BS EN ISO 11970:2016 Specification and qualification of welding procedures for production welding of steel castings
Sponsored link
sklademVydáno: 2016-04-30
BS EN ISO 11970:2016 Specification and qualification of welding procedures for production welding of steel castings

BS EN ISO 11970:2016

Specification and qualification of welding procedures for production welding of steel castings

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
6820 Kč
Čtěte normu po dobu 1 hodiny. Více informací v kategorii E-READING
Čtení normy
na 1 hodinu
682.00 Kč
Čtěte normu po dobu 24 hodin. Více informací v kategorii E-READING
Čtení normy
na 24 hodin
2046.00 Kč
Anglicky Tisk
Skladem
6820 Kč
Označení normy:BS EN ISO 11970:2016
Počet stran:28
Vydáno:2016-04-30
ISBN:978 0 580 76497 4
Status:Standard
Popis

BS EN ISO 11970:2016


This standard BS EN ISO 11970:2016 Specification and qualification of welding procedures for production welding of steel castings is classified in these ICS categories:
  • 77.140.80 Iron and steel castings
  • 25.160.10 Welding processes

This International Standard specifies how a welding procedure specification (WPS) for production welding of steel castings is qualified.

It defines the conditions for the execution of welding procedure qualification tests and the limits of validity of a qualified welding procedure for all practical welding operations within the range of essential variables.

Tests are intended to be carried out in accordance with this International Standard unless additional tests are specified by the purchaser or by agreement between the contracting parties.

This International Standard applies to the arc welding of steel castings. The principles of this International Standard can be applied to other fusion welding processes subject to agreement between the contracting parties.

In the case of specific service, material or manufacturing conditions, tests more comprehensive than those specified by this International Standard can be specified by the purchaser, in order to gain more information, e.g. longitudinal weld tensile tests, bend tests, chemical analyses, ferrite determination in austenitic stainless steels, elongation, Charpy “V” impact tests, and radiography.