BS EN ISO 15612:2018 Specification and qualification of welding procedures for metallic materials. Qualification by adoption of a standard welding procedure specification

BS EN ISO 15612:2018

Specification and qualification of welding procedures for metallic materials. Qualification by adoption of a standard welding procedure specification

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
4020 Kč
Anglicky Tisk
Skladem
4020 Kč
Označení normy:BS EN ISO 15612:2018
Počet stran:14
Vydáno:2019-01-14
ISBN:978 0 539 03589 6
Status:Standard
Popis

BS EN ISO 15612:2018


This standard BS EN ISO 15612:2018 Specification and qualification of welding procedures for metallic materials. Qualification by adoption of a standard welding procedure specification is classified in these ICS categories:
  • 25.160.10 Welding processes

This document:

  • specifies how a user can follow a standard welding procedure specification (SWPS) based on welding procedure qualification tests performed by a different organization;

  • specifies the range for the use of SWPSs in accordance with ISO 15607;

  • specifies the requirements for qualification of welding procedures to be issued as SWPSs; and

  • specifies the requirements for organizations adopting SWPSs.

The use of this document can be restricted by an application standard or a specification.

This document is applicable to welding of steels and aluminium and its alloys (see 4.1).

All new standard welding procedure qualifications are to be carried out in accordance with this document from the date of its issue. However, this document does not invalidate previous standard welding procedure qualifications made to former standards, specifications or previous editions of this document.