Cena s DPH / bez DPH
Hlavní stránka>BS EN ISO 20728:2018 Corrosion of metal and alloys. Determination of resistance of magnesium alloys to stress corrosion cracking
Sponsored link
sklademVydáno: 2018-10-18
BS EN ISO 20728:2018 Corrosion of metal and alloys. Determination of resistance of magnesium alloys to stress corrosion cracking

BS EN ISO 20728:2018

Corrosion of metal and alloys. Determination of resistance of magnesium alloys to stress corrosion cracking

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
4740 Kč
Anglicky Tisk
Skladem
4740 Kč
Označení normy:BS EN ISO 20728:2018
Počet stran:18
Vydáno:2018-10-18
ISBN:978 0 580 91144 6
Status:Standard
Popis

BS EN ISO 20728:2018


This standard BS EN ISO 20728:2018 Corrosion of metal and alloys. Determination of resistance of magnesium alloys to stress corrosion cracking is classified in these ICS categories:
  • 77.060 Corrosion of metals

This document specifies a method for the determination of resistance to stress corrosion cracking (SCC) of magnesium alloys intended for use in structural applications (such as magnesium front end, gearbox and clutch housing units, steering column parts, shift actuators, valve covers and housings, brackets and intake manifold blades, electronic devices, power tools and medical equipment). The method allows determination of the resistance to SCC as a function of the chemical composition, the method of manufacture and heat treatment of magnesium alloys.

The document is applicable to cast and wrought magnesium alloys in the form of castings, semi-finished products, parts and weldments and covers the method of sampling, the types of specimens, the loading procedure, the type of environment and the interpretation of results.

The document allows assessment of the relative performance of materials and products in environments containing chlorides or sulphates, provided that the failure mechanism is not changed, but does not qualify a material or product for service application.