BS EN ISO 305:2019 Plastics. Determination of thermal stability of poly(vinyl chloride), related chlorine-containing homopolymers and copolymers and their compounds. Discoloration method

BS EN ISO 305:2019

Plastics. Determination of thermal stability of poly(vinyl chloride), related chlorine-containing homopolymers and copolymers and their compounds. Discoloration method

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
3780 Kč
Čtěte normu po dobu 1 hodiny. Více informací v kategorii E-READING
Čtení normy
na 1 hodinu
378.00 Kč
Čtěte normu po dobu 24 hodin. Více informací v kategorii E-READING
Čtení normy
na 24 hodin
1134.00 Kč
Anglicky Tisk
Skladem
3780 Kč
Označení normy:BS EN ISO 305:2019
Počet stran:14
Vydáno:2019-06-18
ISBN:978 0 580 92867 3
Status:Standard
Popis

BS EN ISO 305:2019


This standard BS EN ISO 305:2019 Plastics. Determination of thermal stability of poly(vinyl chloride), related chlorine-containing homopolymers and copolymers and their compounds. Discoloration method is classified in these ICS categories:
  • 83.080.20 Thermoplastic materials

This document specifies two methods for the determination of the thermal stability of products and compounds based on vinyl chloride homopolymers and copolymers (referred to simply as PVC in the following text) by the extent of the discoloration that occurs when they are exposed, in the form of sheet, to elevated temperatures. The two methods are:

  • Method A: Oil-bath method;

  • Method B: Oven method.

These methods are particularly applicable to the determination of the resistance of PVC to degradation by heat, as assessed by the change in colour after different times of heating under standardized conditions. The results are comparative only, and can be unsatisfactory when coloured PVC materials are tested.

The stability times given by the two methods might not be similar and cannot be used for direct-comparison purposes.