sklademVydáno: 1995-09-01
BS EN ISO 7539-5:1995 Corrosion of metals and alloys. Stress corrosion testing Method for the preparation and use of C-ring specimens

BS EN ISO 7539-5:1995

Corrosion of metals and alloys. Stress corrosion testing Method for the preparation and use of C-ring specimens

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
4740 Kč
Anglicky Tisk
Skladem
4740 Kč
Označení normy:BS EN ISO 7539-5:1995
Počet stran:18
Vydáno:1995-09-01
ISBN:0 580 18795 0
Status:Standard
Popis

BS EN ISO 7539-5:1995


This standard BS EN ISO 7539-5:1995 Corrosion of metals and alloys. Stress corrosion testing is classified in these ICS categories:
  • 77.060 Corrosion of metals

Procedures for designing, preparing and using C-ring test specimens for investigating the susceptibility of a metal to stress corrosion.