Cena s DPH / bez DPH
Hlavní stránka>BS EN ISO 8994:2018 Anodizing of aluminium and its alloys. Rating system for the evaluation of pitting corrosion. Grid method
Sponsored link
sklademVydáno: 2018-12-19
BS EN ISO 8994:2018 Anodizing of aluminium and its alloys. Rating system for the evaluation of pitting corrosion. Grid method

BS EN ISO 8994:2018

Anodizing of aluminium and its alloys. Rating system for the evaluation of pitting corrosion. Grid method

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
4020 Kč
Anglicky Tisk
Skladem
4020 Kč
Označení normy:BS EN ISO 8994:2018
Počet stran:12
Vydáno:2018-12-19
ISBN:978 0 580 97203 4
Status:Standard
Popis

BS EN ISO 8994:2018


This standard BS EN ISO 8994:2018 Anodizing of aluminium and its alloys. Rating system for the evaluation of pitting corrosion. Grid method is classified in these ICS categories:
  • 25.220.20 Surface treatment
  • 77.060 Corrosion of metals

This document specifies a grid rating system that provides a means of defining levels of performance of anodic oxidation coatings on aluminium and its alloys that have been subjected to corrosion tests.

This rating system is applicable to pitting corrosion resulting from

  • accelerated tests,

  • exposure to corrosive environments, and

  • practical service tests.

This document takes into account only pitting corrosion of the basis metal resulting from penetration of the protective anodic oxidation coating.

NOTE 1 ISO 8993[1] describes a similar rating system based on defined chart scales.

NOTE 2 The grid rating system is frequently used for rating the results of short-term corrosion tests for relatively thin anodic oxidation coating, such as those used in the automotive industry.