Hlavní stránka>BS ISO 10952:2021 - TC Tracked Changes. Glass-reinforced thermosetting plastics (GRP) pipes and fittings. Determination of the resistance to chemical attack for the inside of a section in a deflected condition
Sponsored link
sklademVydáno: 2021-11-09
BS ISO 10952:2021 - TC Tracked Changes. Glass-reinforced thermosetting plastics (GRP) pipes and fittings. Determination of the resistance to chemical attack for the inside of a section in a deflected condition

BS ISO 10952:2021 - TC

Tracked Changes. Glass-reinforced thermosetting plastics (GRP) pipes and fittings. Determination of the resistance to chemical attack for the inside of a section in a deflected condition

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
6882 Kč
Anglicky Tisk
Skladem
6882 Kč
Označení normy:BS ISO 10952:2021 - TC
Počet stran:34
Vydáno:2021-11-09
ISBN:978 0 539 19907 9
Status:Tracked Changes
Popis

BS ISO 10952:2021 - TC


This standard BS ISO 10952:2021 - TC Tracked Changes. Glass-reinforced thermosetting plastics (GRP) pipes and fittings. Determination of the resistance to chemical attack for the inside of a section in a deflected condition is classified in these ICS categories:
  • 23.040.45 Plastics fittings
  • 23.040.20 Plastics pipes

This document specifies a method for determining the chemical resistance properties of glass-reinforced thermosetting plastics (GRP) pipes and fittings in a deflected condition for nominal sizes DN 100 and larger.

In conjunction with ISO 10928, this document provides a method for evaluating the effect of a chemical environment on the interior of a pipe or fitting after a specified period of time. Test conditions and requirements are specified in the referring International Standard. ISO 23856 references this document.

NOTE

It has been found that the effect of chemical environments can be accelerated by strain induced from deflection; hence, this type of effect is frequently referred to as strain corrosion.