Cena s DPH / bez DPH
Hlavní stránka>BS ISO 14848:1998 Plastics. Unsaturated-polyester resins. Determination of reactivity at 130°C
Sponsored link
sklademVydáno: 1998-08-15
BS ISO 14848:1998 Plastics. Unsaturated-polyester resins. Determination of reactivity at 130°C

BS ISO 14848:1998

Plastics. Unsaturated-polyester resins. Determination of reactivity at 130°C

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
3906 Kč
Čtěte normu po dobu 1 hodiny. Více informací v kategorii E-READING
Čtení normy
na 1 hodinu
390.60 Kč
Čtěte normu po dobu 24 hodin. Více informací v kategorii E-READING
Čtení normy
na 24 hodin
1171.80 Kč
Anglicky Tisk
Skladem
3906 Kč
Označení normy:BS ISO 14848:1998
Počet stran:12
Vydáno:1998-08-15
ISBN:0 580 30005 6
Status:Standard
Popis

BS ISO 14848:1998


This standard BS ISO 14848:1998 Plastics. Unsaturated-polyester resins. Determination of reactivity at 130°C is classified in these ICS categories:
  • 83.080.10 Thermosetting materials

This International Standard specifies a method of measuring

  • the time required for the temperature of a solution of unsaturated-polyester resin and a catalyst, heated in a thermostatically controlled bath at 130 °C, to rise

  • from 80 °C to 140 °C,

  • from 80 °C to the maximum temperature reached;

  • the maximum temperature reached;

  • the speed of the reaction, determined by drawing a tangent at the point of inflection of the temperature/time curve.

It applies in particular to unsaturated-polyester resins processed at a temperature higher than 100 °C.

NOTE - The results are closely linked to the conditions. The aim of this International Standard is to define them as exactly as possible, particularly the following:

  1. The quantity and form of the resin sample being examined (test tube diameter, height of resin in the tube).

  2. The rate at which the sample is heated in the bath. For example, the use of a liquid having a relatively low heat capacity (ethylene glycol, silicone oil) leads to slower heating.

  3. The type of thermometer used. Thermometers having a response slower than that of a thermocouple, and resistance probes having too large a heat-sensitive element, are unsuitable.

  4. The position of the heat-sensitive element in the resin, both heightwise and relative to the axis of the test tube containing the resin.

  5. The nature of the catalyst.