Hlavní stránka>BS ISO 18373-1:2007 Rigid PVC pipes. Differential scanning calorimetry (DSC) method Measurement of the processing temperature
Sponsored link
sklademVydáno: 2007-09-28
BS ISO 18373-1:2007 Rigid PVC pipes. Differential scanning calorimetry (DSC) method Measurement of the processing temperature

BS ISO 18373-1:2007

Rigid PVC pipes. Differential scanning calorimetry (DSC) method Measurement of the processing temperature

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
4740 Kč
Anglicky Tisk
Skladem
4740 Kč
Označení normy:BS ISO 18373-1:2007
Počet stran:18
Vydáno:2007-09-28
ISBN:978 0 580 56391 1
Status:Standard
Popis

BS ISO 18373-1:2007


This standard BS ISO 18373-1:2007 Rigid PVC pipes. Differential scanning calorimetry (DSC) method is classified in these ICS categories:
  • 23.040.20 Plastics pipes

This part of ISO 18373 specifies a method for the determination of the processing temperature of rigid PVC pipe samples. The method is based on the measurement of the thermal history using differential scanning calorimetry (DSC) and is suitable for all types of rigid PVC pipes.