BS ISO 21746:2019 Composites and metal assemblies. Galvanic corrosion tests of carbon fibre reinforced plastics (CFRPs) related bonded or fastened structures in artificial atmospheres. Salt spray tests

BS ISO 21746:2019

Composites and metal assemblies. Galvanic corrosion tests of carbon fibre reinforced plastics (CFRPs) related bonded or fastened structures in artificial atmospheres. Salt spray tests

Formát
Dostupnost
Cena a měna
Anglicky Zabezpečené PDF
K okamžitému stažení
6600 Kč
Anglicky Tisk
Skladem
6600 Kč
Označení normy:BS ISO 21746:2019
Počet stran:28
Vydáno:2019-05-03
ISBN:978 0 580 95914 1
Status:Standard
Popis

BS ISO 21746:2019


This standard BS ISO 21746:2019 Composites and metal assemblies. Galvanic corrosion tests of carbon fibre reinforced plastics (CFRPs) related bonded or fastened structures in artificial atmospheres. Salt spray tests is classified in these ICS categories:
  • 83.120 Reinforced plastics

This document specifies the apparatus, the reagents and the procedure to be used in conducting the neutral salt spray (NSS), acetic acid salt spray (AASS) and copper-accelerated acetic acid salt spray (CASS) tests for assessment of the galvanic corrosion resistance of joints and bonded structures between carbon fibre reinforced plastics (CFRPs) and metallic materials, with or without permanent or temporary insulation for the galvanic current.