Menu
0
Total price
0 €
PRICES include / exclude VAT
Homepage>BS 6783-1:1986 Sampling and analysis of nickel, ferronickel and nickel alloys Method for determination of silver, bismuth, cadmium, cobalt, copper, iron, manganese, lead and zinc in nickel by flame atomic absorption spectrometry
Sponsored link
sklademVydáno: 1986-12-31
BS 6783-1:1986 Sampling and analysis of nickel, ferronickel and nickel alloys Method for determination of silver, bismuth, cadmium, cobalt, copper, iron, manganese, lead and zinc in nickel by flame atomic absorption spectrometry

BS 6783-1:1986

Sampling and analysis of nickel, ferronickel and nickel alloys Method for determination of silver, bismuth, cadmium, cobalt, copper, iron, manganese, lead and zinc in nickel by flame atomic absorption spectrometry

Format
Availability
Price and currency
Anglicky Secure PDF
Immediate download
183.40 €
You can read the standard for 1 hour. More information in the category: E-reading
Reading the standard
for 1 hour
18.34 €
You can read the standard for 24 hours. More information in the category: E-reading
Reading the standard
for 24 hours
55.02 €
Anglicky Hardcopy
In stock
183.40 €
Označení normy:BS 6783-1:1986
Počet stran:16
Vydáno:1986-12-31
ISBN:0 580 15520 X
Status:Standard
DESCRIPTION

BS 6783-1:1986


This standard BS 6783-1:1986 Sampling and analysis of nickel, ferronickel and nickel alloys is classified in these ICS categories:
  • 77.120.40 Nickel, chromium and their alloys

This International Standard specifies a flame atomic absorption spectrometric method for the determination of the silver, bismuth, cadmium, cobalt, copper, iron, manganese, lead and zinc contents of refined, wrought and cast nickel within the ranges specified in Table 1. This method is applicable to the independent determination of any one or more of the elements listed without including all the elements specified in the standard solutions.

Table 1 – Concentration ranges of elements to be determined

Element Concentration range, [% (m/m)]a
Procedure A Procedure B
Ag 0,000 2 to 0,01
Bi 0,000 1 to 0,01
Cd 0,000 2 to 0,002 5
Co 0,001 0 to 0,01 to 1,00
Cu 0,000 2 to 0,01 0,01 to 1,00
Fe 0,002 5 to 0,01 0,01 to 0,15
Mn 0,000 5 to 0,01 0,01 to 0,20
Pb 0,000 5 to 0,01
Zn 0,000 2 to 0,002 5 0,00 1 to 0,01 5
a For specific compositions, see ISO 6283.

The lower level for iron can be extended to less than 0,002 5 % (m/m) provided nickel containing less than 0,000 1 % (m/m) iron is used for preparation of standard solutions; see 4.1.

The upper limit for the determination of cobalt and copper can be raised to 2 % (m/m) by a minor modification to the method; see 11.1.

For potential interferences, see clause 10.