Menu
0
Total price
0 €
PRICES include / exclude VAT
Homepage>BS EN 10025-6:2019+A1:2022 Hot rolled products of structural steels Technical delivery conditions for flat products of high yield strength structural steels in the quenched and tempered condition
Sponsored link
sklademVydáno: 2023-04-12
BS EN 10025-6:2019+A1:2022 Hot rolled products of structural steels Technical delivery conditions for flat products of high yield strength structural steels in the quenched and tempered condition

BS EN 10025-6:2019+A1:2022

Hot rolled products of structural steels Technical delivery conditions for flat products of high yield strength structural steels in the quenched and tempered condition

Format
Availability
Price and currency
Anglicky Secure PDF
Immediate download
254.31 €
You can read the standard for 1 hour. More information in the category: E-reading
Reading the standard
for 1 hour
25.43 €
You can read the standard for 24 hours. More information in the category: E-reading
Reading the standard
for 24 hours
76.29 €
Anglicky Hardcopy
In stock
254.31 €
Označení normy:BS EN 10025-6:2019+A1:2022
Počet stran:32
Vydáno:2023-04-12
ISBN:978 0 539 20756 9
Status:Standard
DESCRIPTION

BS EN 10025-6:2019+A1:2022


This standard BS EN 10025-6:2019+A1:2022 Hot rolled products of structural steels is classified in these ICS categories:
  • 77.140.10 Heat-treatable steels
  • 77.140.50 Flat steel products and semi-products
  • 91.100.99 Other construction materials
This document specifies technical delivery conditions for flat products of high yield strength alloy special steels. The grades and qualities are given in Tables 1 to 3 (chemical composition) and Tables 4 to 6 (mechanical properties) and are supplied in the quenched and tempered condition. The steels specified in this document are applicable to hot-rolled flat products with a minimum nominal thickness of 3 mm and a maximum nominal thickness of 200 mm for grades S460, S500, S550, S620 and S690, a maximum nominal thickness of 125 mm for grades S890 and S960, in steels which, after quenching and tempering, have a specified minimum yield strength of 460 MPa to 960 MPa.