Homepage>BS EN 1011-5:2003 Welding. Recommendations for welding of metallic materials Welding of clad steel
Sponsored link
sklademVydáno: 2003-05-02
BS EN 1011-5:2003 Welding. Recommendations for welding of metallic materials Welding of clad steel

BS EN 1011-5:2003

Welding. Recommendations for welding of metallic materials Welding of clad steel

Format
Availability
Price and currency
Anglicky Secure PDF
Immediate download
166.06 €
You can read the standard for 1 hour. More information in the category: E-reading
Reading the standard
for 1 hour
16.61 €
You can read the standard for 24 hours. More information in the category: E-reading
Reading the standard
for 24 hours
49.82 €
Anglicky Hardcopy
In stock
166.06 €
Označení normy:BS EN 1011-5:2003
Počet stran:14
Vydáno:2003-05-02
ISBN:0 580 41755 7
Status:Standard
DESCRIPTION

BS EN 1011-5:2003


This standard BS EN 1011-5:2003 Welding. Recommendations for welding of metallic materials is classified in these ICS categories:
  • 25.160.10 Welding processes

This European Standard gives general recommendations for welding of clad steels by means of appropriate arc welding processes and electroslag strip cladding.

It is generally applicable to all clad steels and is appropriate regardless of the type of fabrication involved, although the application standard may have additional requirements. Non-ferrous claddings, such as titanium, tantalum, zirconium and their alloys are not covered by this standard.

Examples for joint preparation are given in EN ISO 9692-4.

This standard covers welding of cladding deposits as well as welding of the transition zone(s), when existing, between parent metal and cladding. These transition zones are metal combinations of non-alloyed ferrous parent metal with high alloyed stainless steels, nickel alloys or other non-ferrous metals.

The mechanical and physical design of the joints is not covered by this standard. Methods of testing and acceptance levels are not included because they depend on the service conditions of the fabrication. These details should be obtained from the design specification.

The corrosion resistance of the cladding depends on many factors and is not a part of this standard.