BS EN 14179-1:2016 Glass in building. Heat soaked thermally toughened soda lime silicate safety glass Definition and description

BS EN 14179-1:2016

Glass in building. Heat soaked thermally toughened soda lime silicate safety glass Definition and description

Format
Availability
Price and currency
Anglicky Secure PDF
Immediate download
337.45 €
You can read the standard for 1 hour. More information in the category: E-reading
Reading the standard
for 1 hour
33.75 €
You can read the standard for 24 hours. More information in the category: E-reading
Reading the standard
for 24 hours
101.24 €
Anglicky Hardcopy
In stock
337.45 €
Označení normy:BS EN 14179-1:2016
Počet stran:50
Vydáno:2016-08-31
ISBN:978 0 580 87502 1
Status:Standard
DESCRIPTION

BS EN 14179-1:2016


This standard BS EN 14179-1:2016 Glass in building. Heat soaked thermally toughened soda lime silicate safety glass is classified in these ICS categories:
  • 81.040.20 Glass in building

This European Standard specifies the heat soak process system together with tolerances, flatness, edgework, fragmentation and physical and mechanical characteristics of monolithic flat heat soaked thermally toughened soda lime silicate safety glass for use in buildings.

Curved heat soaked thermally toughened soda lime silicate safety glass is not part of this European Standard.

Other requirements, not specified in this European Standard, can apply to heat soaked thermally toughened soda lime silicate safety glass which is incorporated into assemblies, e.g. laminated glass or insulating units, or undergo an additional treatment, e.g. coating. The additional requirements are specified in the appropriate product standard. Heat soaked thermally toughened soda lime silicate safety glass, in this case, does not lose its bending strength characteristics and its resistance to temperature differentials.

Surface finished glasses (e.g. sandblasted, acid etched) after toughening are not covered by this European Standard.