Vážení zákazníci, v letošním roce budeme expedovat poslední objednávky ve středu 18. 12. 2024.

Těšíme se s vámi na shledanou od pondělí 06. 01. 2025.

 

Menu
0
Total price
0 €
PRICES include / exclude VAT
Homepage>BS EN 15384-2:2017 Packaging. Test method to determine the porosity of the internal coating of flexible aluminium tubes Copper sulphate test
Sponsored link
sklademVydáno: 2017-02-28
BS EN 15384-2:2017 Packaging. Test method to determine the porosity of the internal coating of flexible aluminium tubes Copper sulphate test

BS EN 15384-2:2017

Packaging. Test method to determine the porosity of the internal coating of flexible aluminium tubes Copper sulphate test

Format
Availability
Price and currency
Anglicky Secure PDF
Immediate download
164.81 €
You can read the standard for 1 hour. More information in the category: E-reading
Reading the standard
for 1 hour
16.48 €
You can read the standard for 24 hours. More information in the category: E-reading
Reading the standard
for 24 hours
49.44 €
Anglicky Hardcopy
In stock
164.81 €
Označení normy:BS EN 15384-2:2017
Počet stran:12
Vydáno:2017-02-28
ISBN:978 0 580 91014 2
Status:Standard
DESCRIPTION

BS EN 15384-2:2017


This standard BS EN 15384-2:2017 Packaging. Test method to determine the porosity of the internal coating of flexible aluminium tubes is classified in these ICS categories:
  • 55.120 Cans. Tins. Tubes

This European Standard is applicable for internally coated cylindrical aluminium tubes, mainly used for the packing of pharmaceutical, cosmetic, hygiene, food or other household products.

The internal coating is used as a barrier and should avoid any contact between aluminium and the product. This standard defines the copper sulphate method to detect the electrolyte conductivity as one criterion for the quality of the internal coating.

The electrolyte conductivity of the internal coating is only one criterion for evaluation of the quality of an internal coating. It does not give any information on the quantity or size of any pores or uncoated areas, nor any hint on possible reactions between the aluminium tube and the product. The electrolyte conductivity should never be used as the sole criterion for quality evaluation of the internal coating, but always with other parameters e.g. film thickness, acetone and/or ammonia resistance and of course results of enhanced stability studies.