Homepage>BS EN ISO 15610:2024 Specification and qualification of welding procedures for metallic materials. Qualification based on tested welding consumables
Sponsored link
sklademVydáno: 2024-03-20
BS EN ISO 15610:2024 Specification and qualification of welding procedures for metallic materials. Qualification based on tested welding consumables

BS EN ISO 15610:2024

Specification and qualification of welding procedures for metallic materials. Qualification based on tested welding consumables

Format
Availability
Price and currency
Anglicky Secure PDF
Immediate download
189.52 €
Anglicky Hardcopy
In stock
189.52 €
Označení normy:BS EN ISO 15610:2024
Počet stran:16
Vydáno:2024-03-20
ISBN:978 0 539 27056 3
Status:Standard
DESCRIPTION

BS EN ISO 15610:2024


This standard BS EN ISO 15610:2024 Specification and qualification of welding procedures for metallic materials. Qualification based on tested welding consumables is classified in these ICS categories:
  • 25.160.10 Welding processes
  • 25.030 Additive manufacturing
This document specifies how a welding procedure can be qualified by using tested welding consumable data. It expands on the requirements given in ISO 15607. In addition, it gives the range of qualification. Application of this document is limited to parent material groups 1.1, 8.1, 21, 22.1 and 22.2 in accordance with ISO/TR 15608, which produce acceptable microstructures and properties in the heat-affected zone which do not deteriorate significantly in service. This document is limited to: —     butt welds and fillet welds in material of thicknesses t ? 40 mm (groups 1.1 and 8.1) and t ? 20 mm (groups 21, 22.1 and 22.2); —     fillet welds with throat thickness a ? 1 mm. This document is not applicable when any of the following is specified for the welded joint: a)       hardness; b)       impact properties; c)        preheating; d)       controlled heat input; e)       interpass temperature; f)         post-weld heat treatment. The use of this document can also be restricted by an application standard, specification or other documents.