Menu
0
Total price
0 €
PRICES include / exclude VAT
Homepage>BS EN ISO 20728:2018 Corrosion of metal and alloys. Determination of resistance of magnesium alloys to stress corrosion cracking
Sponsored link
sklademVydáno: 2018-10-18
BS EN ISO 20728:2018 Corrosion of metal and alloys. Determination of resistance of magnesium alloys to stress corrosion cracking

BS EN ISO 20728:2018

Corrosion of metal and alloys. Determination of resistance of magnesium alloys to stress corrosion cracking

Format
Availability
Price and currency
Anglicky Secure PDF
Immediate download
194.87 €
You can read the standard for 1 hour. More information in the category: E-reading
Reading the standard
for 1 hour
19.49 €
You can read the standard for 24 hours. More information in the category: E-reading
Reading the standard
for 24 hours
58.46 €
Anglicky Hardcopy
In stock
194.87 €
Označení normy:BS EN ISO 20728:2018
Počet stran:18
Vydáno:2018-10-18
ISBN:978 0 580 91144 6
Status:Standard
DESCRIPTION

BS EN ISO 20728:2018


This standard BS EN ISO 20728:2018 Corrosion of metal and alloys. Determination of resistance of magnesium alloys to stress corrosion cracking is classified in these ICS categories:
  • 77.060 Corrosion of metals

This document specifies a method for the determination of resistance to stress corrosion cracking (SCC) of magnesium alloys intended for use in structural applications (such as magnesium front end, gearbox and clutch housing units, steering column parts, shift actuators, valve covers and housings, brackets and intake manifold blades, electronic devices, power tools and medical equipment). The method allows determination of the resistance to SCC as a function of the chemical composition, the method of manufacture and heat treatment of magnesium alloys.

The document is applicable to cast and wrought magnesium alloys in the form of castings, semi-finished products, parts and weldments and covers the method of sampling, the types of specimens, the loading procedure, the type of environment and the interpretation of results.

The document allows assessment of the relative performance of materials and products in environments containing chlorides or sulphates, provided that the failure mechanism is not changed, but does not qualify a material or product for service application.