Homepage>BS EN ISO 7539-1:2012 Corrosion of metals and alloys. Stress corrosion testing General guidance on testing procedures
Sponsored link
sklademVydáno: 2013-01-31
BS EN ISO 7539-1:2012 Corrosion of metals and alloys. Stress corrosion testing General guidance on testing procedures

BS EN ISO 7539-1:2012

Corrosion of metals and alloys. Stress corrosion testing General guidance on testing procedures

Format
Availability
Price and currency
Anglicky Secure PDF
Immediate download
272.69 €
You can read the standard for 1 hour. More information in the category: E-reading
Reading the standard
for 1 hour
27.27 €
You can read the standard for 24 hours. More information in the category: E-reading
Reading the standard
for 24 hours
81.81 €
Anglicky Hardcopy
In stock
272.69 €
Označení normy:BS EN ISO 7539-1:2012
Počet stran:30
Vydáno:2013-01-31
ISBN:978 0 580 71187 9
Status:Standard
DESCRIPTION

BS EN ISO 7539-1:2012


This standard BS EN ISO 7539-1:2012 Corrosion of metals and alloys. Stress corrosion testing is classified in these ICS categories:
  • 77.060 Corrosion of metals

1.1 This part of ISO 7539 describes the general considerations that apply when designing and conducting tests to assess susceptibility of metals to stress corrosion.

1.2 This part of ISO 7539 also gives some general guidance on the selection of test methods.

NOTE 1 Particular methods of test are not treated in detail in this part of ISO 7539. These are described in the additional parts of ISO 7539.

NOTE 2 This part of ISO 7539 is applicable to cathodic protection conditions.