BS EN ISO 7539-10:2020
Corrosion of metals and alloys. Stress corrosion testing Reverse U-bend method
Format
Availability
Price and currency
Anglicky Secure PDF
Immediate download
195.18 €
You can read the standard for 1 hour. More information in the category: E-reading
Reading the standardfor 1 hour
19.52 €
You can read the standard for 24 hours. More information in the category: E-reading
Reading the standardfor 24 hours
58.55 €
Anglicky Hardcopy
In stock
195.18 €
Označení normy: | BS EN ISO 7539-10:2020 |
Počet stran: | 22 |
Vydáno: | 2020-06-03 |
ISBN: | 978 0 539 03076 1 |
Status: | Standard |
DESCRIPTION
BS EN ISO 7539-10:2020
This standard BS EN ISO 7539-10:2020 Corrosion of metals and alloys. Stress corrosion testing is classified in these ICS categories:
- 77.060 Corrosion of metals
This document specifies procedures for designing, preparing and using reversed U-bend (RUB) test specimens for investigating the susceptibility of the metal to stress corrosion cracking. The term “ metal” as used in this document includes alloys.