BS ISO 15309:2013 Implants for surgery. Differential scanning calorimetry of poly ether ether ketone (PEEK) polymers and compounds for use in implantable medical devices

BS ISO 15309:2013

Implants for surgery. Differential scanning calorimetry of poly ether ether ketone (PEEK) polymers and compounds for use in implantable medical devices

Format
Availability
Price and currency
Anglicky Secure PDF
Immediate download
189.52 €
Anglicky Hardcopy
In stock
189.52 €
Označení normy:BS ISO 15309:2013
Počet stran:18
Vydáno:2013-12-31
ISBN:978 0 580 74909 4
Status:Standard
DESCRIPTION

BS ISO 15309:2013


This standard BS ISO 15309:2013 Implants for surgery. Differential scanning calorimetry of poly ether ether ketone (PEEK) polymers and compounds for use in implantable medical devices is classified in these ICS categories:
  • 11.040.40 Implants for surgery, prosthetics and orthotics

This International Standard specifies a method for the thermal analysis of Poly Ether Ether Ketone (PEEK) that is for use in the manufacture of implantable medical devices, using differential scanning calorimetry (DSC).

The transition temperatures to be determined are the glass transition temperature (Tg), the melting temperature (Tm) and the crystallization temperature on cooling (Tc).