BS ISO 16540:2015 Corrosion of metals and alloys. Methodology for determining the resistance of metals to stress corrosion cracking using the four-point bend method

BS ISO 16540:2015

Corrosion of metals and alloys. Methodology for determining the resistance of metals to stress corrosion cracking using the four-point bend method

Format
Availability
Price and currency
Anglicky Secure PDF
Immediate download
272.69 €
You can read the standard for 1 hour. More information in the category: E-reading
Reading the standard
for 1 hour
27.27 €
You can read the standard for 24 hours. More information in the category: E-reading
Reading the standard
for 24 hours
81.81 €
Anglicky Hardcopy
In stock
272.69 €
Označení normy:BS ISO 16540:2015
Počet stran:30
Vydáno:2015-10-31
ISBN:978 0 580 73641 4
Status:Standard
DESCRIPTION

BS ISO 16540:2015


This standard BS ISO 16540:2015 Corrosion of metals and alloys. Methodology for determining the resistance of metals to stress corrosion cracking using the four-point bend method is classified in these ICS categories:
  • 77.060 Corrosion of metals

This International Standard provides guidelines for the use of four-point bend testing to evaluate the resistance of metals including carbon steel, low alloy steels, and corrosion resistant alloys (CRAs) to stress corrosion cracking. The method gives guidance on testing of both parent plate and welds and includes procedures for metals that have no distinct yield point in their stress-strain behaviour as well as metals with a distinct yield point. The emphasis in this International Standard is on the generic methodology of the four-point bend test. Service application will be varied and the relevant industry standard is to be consulted where appropriate.