PRICES include / exclude VAT
Sponsored link
sklademVydáno: 2021-02-24
BS ISO 22848:2021
Corrosion of metals and alloys. Test method for measuring the stress corrosion crack growth rate of steels and alloys under static-load conditions in high-temperature water
Format
Availability
Price and currency
Anglicky Secure PDF
Immediate download
273.18 €
You can read the standard for 1 hour. More information in the category: E-reading
Reading the standardfor 1 hour
27.32 €
You can read the standard for 24 hours. More information in the category: E-reading
Reading the standardfor 24 hours
81.95 €
Anglicky Hardcopy
In stock
273.18 €
Označení normy: | BS ISO 22848:2021 |
Počet stran: | 32 |
Vydáno: | 2021-02-24 |
ISBN: | 978 0 580 51813 3 |
Status: | Standard |
DESCRIPTION
BS ISO 22848:2021
This standard BS ISO 22848:2021 Corrosion of metals and alloys. Test method for measuring the stress corrosion crack growth rate of steels and alloys under static-load conditions in high-temperature water is classified in these ICS categories:
- 77.060 Corrosion of metals
This document specifies a test method for determining the stress corrosion crack (SCC) growth rate of steels and alloys under static-load conditions in high-temperature water, such as the simulated water environment of light water reactors. The crack length of the specimen is monitored by a potential drop method (PDM) during the test in an autoclave.
The test method is applicable to stainless steels, nickel base alloys, low alloy steels, carbon steels and other alloys.