ISO 21746:2019-Composites and metal assemblies — Galvanic corrosion tests of carbon fibre reinforced plastics (CFRPs) related bonded or fastened structures in artificial atmospheres — Salt spray tests
Format
Availability
Price and currency
Anglicky PDF
Immediate download
158.93 €
Anglicky Hardcopy
In stock
158.93 €
Označení normy: | ISO 21746:2019 |
Počet stran: | 19 |
Vydání: | 1 |
Vydáno: | 2019 |
Jazyk: | Anglicky |
DESCRIPTION
ISO 21746:2019
This document specifies the apparatus, the reagents and the procedure to be used in conducting the neutral salt spray (NSS), acetic acid salt spray (AASS) and copper-accelerated acetic acid salt spray (CASS) tests for assessment of the galvanic corrosion resistance of joints and bonded structures between carbon fibre reinforced plastics (CFRPs) and metallic materials, with or without permanent or temporary insulation for the galvanic current.