Cena s DPH / bez DPH
Sponsored link
sklademVydáno: 1989
ISO 7539-2:1989
ISO 7539-2:1989-Corrosion of metals and alloys — Stress corrosion testing-Part 2: Preparation and use of bent-beam specimens
Formát
Dostupnost
Cena a měna
Anglicky PDF
K okamžitému stažení
1800 Kč
Francouzsky PDF
K okamžitému stažení
1800 Kč
Anglicky Tisk
Skladem
1800 Kč
Francouzsky Tisk
Skladem
1800 Kč
Označení normy: | ISO 7539-2:1989 |
Počet stran: | 6 |
Vydání: | 1 |
Vydáno: | 1989 |
Popis
ISO 7539-2:1989
Covers procedures for designing, preparing and using bent-beam test specimens. These specimens may be used to test a variety of product forms (i. e. sheet, plate, flat extruded material, wire or rod). They are espesially suitable for multiple testing and for atmospheric stress corrosion tests; they are usually tested under nominally constant strain conditions. Bent-beam specimens made from high strength materials may fracture rapidly and can be dangerous.